Standard

ASTM A240, EN 10088-2, GB/T 3280

Grad

1.4372, SUS201, X12CrMnNiN17-7-5, Z12CMN17-07Az

Tul

2000 mm-6000 mm (78.74-236.22 pulzieri), Personalizzat

Wisa' Sħiħ

1000 mm-2000 mm (39.37-78.74 in), Personalizzat

Ħxuna

0.3 mm-6 mm (0.012-0.24 in), Personalizzata

Finish tal-wiċċ

2B, 8K, BA, eċċ., HL, No.1, No.4

Teknika

Cold Drawn, Cold Rolled, Hot Rolled

Formola

Coil, Folja rrumblata kiesħa, Folji intaljati, eċċ., Pjanċa ċatta & Folja, Folja rrumblata bis-sħana, Folji mtaqqba, Pjanċa, Folji illustrati, Strixxa, Folji b'tessut

 

Kompożizzjonijiet Kimiċi

Element Karbonju (C) Manganiż (Mn) Silikon (Si) Fosfru (P) Kubrit (S) Kromju (Cr) Nikil (Ni) Nitroġenu (N)
                 
Kompożizzjoni (%) 0.15 max 5.5-7.5 1.0 max 0.06 max 0.03 max 16.0-18.0 3.5-5.5 0.25 max

Proprjetajiet Mekkaniċi

Proprjetajiet Unità Metrika Unità Imperjali
     
Qawwa tat-tensjoni 655 – 860 MPa 95 – 125 ksi
Qawwa tar-Rendiment 450 MPa 65 ksi
Ebusija Vickers 230 – 270 HV 230 – 270 HV
Ebusija Brinell 200 – 250 HB 200 – 250 HB
Ebusija Rockwell 50 – 56 HRC 50 – 56 HRC
Titwil 20% 20%
Modulu Elastiku 200 GPa 29 x 10^6 psi