2507 Stainless Steel Grad

Mar 23, 2026

Ħalli messaġġ

304L Stainless Steel Pipe for Nuclear Power Auxiliary Systems304L Stainless Steel Coil for Petrochemical Pipelines304L Stainless Steel Sheet for Chemical Tank Linings

 

Proprjetajiet Kimiċi

Valuri tipiċi (Piż %)

C Cr Ni Mo N Oħrajn
0.020 25 7 4.0 0.27 S=0.001

Proprjetajiet Mekkaniċi

Qawwa tat-tensjoni Ultimate, ksi 116 min.
0.2% Offset Yield Strength 0.2%, ksi 80 min.
0.1% Offset Yield Strength 0.2%, ksi 91 min.
Titwil f'2 pulzieri, % 15 min.
Ebusija Rockwell C 32 max.
Enerġija tal-Impatt, ft.-lbs. 74 min.

Proprjetajiet Fiżiċi

Densità lb/in^3 0.28
Modulu ta 'Elastiċità psi x 10^6 29
Koeffiċjent ta 'Espansjoni Termali
68-212 grad F/ grad F
x10^-6/ grad F 7.2
Konduttività Termali Btu/h ft grad F 8.7
Kapaċità tas-Sħana Btu/lb/grad F 0.12
Reżistenza Elettrika W-f'x 10^-6 31.5