Folja tal-metall tal-azzar li ma jsaddadx 304L / 2B
Feb 24, 2026
Ħalli messaġġ




Daqs: 1000x2000mm 1219x2438mm ieħor għandna kolji fl-istokk, nistgħu naqtgħuha għal kwalunkwe tul kif meħtieġ mill-klijent.
Wisa 'ta' tagħna coil tarf mil: 1020-1050mm 1220-1265mm
ħxuna: 0.3-3.0mm
Kompożizzjoni Kimika
|
azzar li ma jissaddadx |
C |
Mn |
P |
S |
Si |
Cr |
Ni |
|
304 |
0.08 max |
2.0 max |
0.045 max |
0.030 max |
1.5 max |
18.0 - 20.0 |
8.0 - 10.0 |
|
304L |
0.03 max |
2.0 max |
0.045 max |
0.030 max |
1.5 max |
18.0 - 20.0 |
8.0 - 10.0 |
.
Proprjetajiet mekkaniċi f'temperatura tal-kamra
|
|
azzar li ma jissaddadx 304 |
azzar li ma jissaddadx 304L |
||
|
|
Tipiku |
Minimu |
Tipiku |
Minimu |
|
Qawwa tat-tensjoni, MPa |
625 |
515 |
575 |
515 |
|
Stress tar-Rendiment (0.2 % offset), MPa |
350 |
205 |
290 |
205 |
|
Titwil (Perċentwal f'50mm) |
50 |
40 |
50 |
40 |
|
Ebusija (Brinell) |
172 |
- |
156 |
- |
|
Limitu ta' reżistenza (għeja), MPa |
260 |
- |
260 |
- |
dettalji tal-ippakkjar
ippakkjar: pakkjar standard għall-esportazzjoni jew kif meħtieġ.
kaxxa tal-injam magħquda jew tkun meħtieġa; Id-daqs ta 'ġewwa tal-kontenitur huwa hawn taħt: 20 pied GP: 5.8m (tul) x 2.13m (wisa') x 2.18m (għoli) madwar 24-26 CBM 40 pied GP: 11.8m (tul) x 2.13m (wisa ') x 2.72m (għoli) madwar CBMabout
Ibgħat l-inkjesta