304L Stainless Steel Welding Wajer Grad
Feb 26, 2026
Ħalli messaġġ



304/304L/304H Stainless Steel Wajer Kompożizzjoni Kimika
| Grad | C | Mn | Si | P | S | Cr | Mo |
| Alloy Steel F11 | 0.05-0.15 | 0.3-0.6 | 0.5-1 | 0.03 | 0.03 | 1-1.5 | 0.44-0.65 |
Stainless Steel 304/304L/304H Wajer Proprjetajiet Mekkaniċi
| Qawwa tat-tensjoni | Qawwa tar-Rendiment (0.2% Offset) | Titwil |
| 205 | 415 | 20 % |
Gradi Ekwivalenti għal Wajer tal-Azzar Stainless 304/304L/304H
| Grad | UNS Nru | Ingliżi qodma | Ewronorma | Svediż SS | JIS Ġappuniż | ||
| BS | En | Nru | Isem | ||||
| 304 | S30400 | 304S31 | 58E | 1.4301 | X5CrNi18-10 | 2332 | SUS 304 |
| 304L | S30403 | – | – | 1.4306/1.4307 | – | – | SUS 304L |
| 304H | S30409 | – | – | 1.4301 | – | – | – |
Li jmiss: 410 Stainless Steel - Grad Martensitiku
Ibgħat l-inkjesta