316L Stainless Steel Folja 1.0mm Cold Rolled ASTM A240 DIN1.4404

Mar 23, 2026

Ħalli messaġġ

What is 1.4537 Stainless Steel?What is 1.4529 Stainless Steel?Stainless Steel - Grade 440 (UNS S44000)

Tip Folja tal-Azzar Stainless
Grad 200 Serje:201/202
300 Serje: 301/302/303/304/304 L/304 N/309/309 S/310/316/316 L/321/347
400 Serje: 403/408/409/410/416/420/430/431/440/440A/440B/440C/439/443/444
600 Serje: 610/620/630
Serje 900: 904L
Ħxuna 0.3-100mm
Wisa' 600mm, 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, eċċ
Tul 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, eċċ
Wiċċ BA/2B/NO.1/NO.4/8K/HL
Test tal-kwalità nistgħu noffru MTC, ISO, SGS, BV, eċċ
Termini tal-ħlas L/CT/T (30% DEPOŻITU)
Stokk jew le Stokk biżżejjed
Kampjun Kampjun Ħieles
Applikazzjoni Industrija tal-kimika,Strument mediku,Materjal tal-kostruzzjoni,Dekorattivi,
Oġġetti tal-kċina, Ikel, eċċ
Ħin tal-kunsinna Fi żmien 7-15-il jum

 

 

Gradi Ekwivalenti ta 'A240 Stainless Steel 316L Sheets & Plates

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR MT
SS 316L 1.4404/1.4435 S31603 SUS 316L 316S11/316S13 03Ch17N14M3 / 03Ch17N14M2 Z3CND17-11-02 / Z3CND18-14-03 X2CrNiMo17-12-2 / X2CrNiMo18-14-3

Stainless Steel 316L Sheets & Plates Proprjetajiet Kimiċi

Grad C Mn Si P S Cr Mo Ni N
SS 316L 0.035 max 2.0 max 1.00 max 0.045 max 0.030 max 16 – 18 2 – 3 10 – 14 68.89 min

SS 316L Sheets & Plates Properties Mechanical

Densità Punt tat-tidwib Qawwa tat-tensjoni Qawwa tar-Rendiment (0.2% Offset) Titwil
8.0 g/ċm3 1399 grad (2550 grad F) Psi – 75000, MPa – 515 Psi – 30000, MPa – 205 35 %

Ibgħat l-inkjesta