420 Prodotti Stainless Steel
Mar 23, 2026
Ħalli messaġġ



Kompożizzjonijiet Kimiċi
|
Element |
C (Karbonju) |
Cr (Kromju) |
Mn (Manganiż) |
Si (silikon) |
P (Fosfru) |
S (kubrit) |
Ni (nikil) |
Ħadid (Fe) |
Ħadid (Fe) |
|---|---|---|---|---|---|---|---|---|---|
| Kontenut | 0.15% – 0.40% | 12.0% – 14.0% | 1.0% max | 1.0% max | 0.04% max | 0.03% max | 0.75% max | Bilanċ | \ |
Proprjetajiet Mekkaniċi
|
Proprjetajiet |
Unità Metrika |
Unità Imperjali |
|---|---|---|
| Qawwa tat-tensjoni | 655 – 860 MPa | 95 – 125 ksi |
| Qawwa tar-Rendiment | 450 MPa | 65 ksi |
| Ebusija Vickers | 230 – 270 HV | 230 – 270 HV |
| Ebusija Brinell | 200 – 250 HB | 200 – 250 HB |
| Ebusija Rockwell | 50 – 56 HRC | 50 – 56 HRC |
| Titwil | 20% | 20% |
| Modulu Elastiku | 200 GPa | 29 x 10^6 psi |
Par ta ' l-:304L Stainless Steel Prodotti
Ibgħat l-inkjesta