Tubu ta 'l-istainless steel ittemprat qawwi ASTM A269 TP316 huwa pajp ta' l-istainless steel awstenitiku magħmul minn materjal TP316 (UNS S31600) u pproċessat minn Bright Annealing (BA). Tipikament fih 16-18% kromju (Cr), 10-14% nikil (Ni), u 2-3% molibdenu (Mo), li jipprovdu reżistenza għall-korrużjoni eċċellenti, finitura għolja tal-wiċċ, u proprjetajiet mekkaniċi tajbin.
Skont ir-rekwiżiti standard, it-tubi tal-istainless steel 316L huma ġeneralment fornuti f'kundizzjoni ta' soluzzjoni-ittemprat. It-temperatura ta 'l-ittemprar mhix inqas minn 1040 grad, segwita minn tkessiħ ta' l-ilma jew tkessiħ rapidu biex tiżgura mikrostruttura uniformi u reżistenza mtejba għall-korrużjoni intergranulari. Il-prodott huwa disponibbli kemm f'forom mingħajr saldatura kif ukoll iwweldjati, b'dijametri ta 'barra komuni li jvarjaw minn 6–48 mm (madwar 1/4"–2") u ħxuna tal-ħajt minn 0.5–3.0 mm. Tulijiet standard jinkludu 3 m, 6 m, jew daqsijiet personalizzati. Il-wiċċ għandu tleqqija metallika tal-fidda-abjad (finitura BA), mingħajr pickling, li fiha ħitan ta 'ġewwa u ta' barra lixxi bi ħruxija baxxa, li jagħmilha faċli biex tnaddaf u sterilizza.



Tubi ASTM A269 TP316 huwa adattat għal applikazzjonijiet b'dijametru ta 'ġewwa akbar minn jew ugwali għal 1/4 pulzier u ħxuna tal-ħajt Akbar minn jew ugwali għal 0.020 pulzier. Huwa użat ħafna fil-kimika, l-ikel, il-farmaċewtika, il-ġenerazzjoni tal-enerġija, iskambjatur tas-sħana, u sistemi ta 'pajpijiet ta' strumentazzjoni fejn huma meħtieġa indafa għolja u reżistenza għall-korrużjoni.
Kompożizzjoni Kimika (ASTM A269 TP316)
| Element | Simbolu | Kontenut (%) |
| Karbonju | C | Inqas minn jew ugwali għal 0.08 |
| Manganiż | Mn | Inqas minn jew ugwali għal 2.00 |
| Fosfru | P | Inqas minn jew ugwali għal 0.045 |
| Kubrit | S | Inqas minn jew ugwali għal 0.030 |
| Silikon | Si | Inqas minn jew ugwali għal 0.75 |
| Kromju | Cr | 16.0 – 18.0 |
| Nikil | Ni | 11.0 – 14.0 |
| Molibdenu | Mo | 2.00 – 3.00 |
sa 269 tp 316 tubu mingħajr saldatura proprjetajiet mekkaniċi
| grad | rendiment str (0.2% prova) (mpa) minimu | tensile str (mpa) minimu | tawwal (% f'50mm) minimu | ebusija rockwell b (hr b) massimu | brinell (hb) massimu |
|---|---|---|---|---|---|
| 316 | 205 | 515 | 40 | 95 | 217 |
proprjetajiet fiżiċi tat-tubi astm a269m tp316
| grad | modulu elastiku (gpa) | densità (kg/meter3) | ko-eff medju ta' espansjoni termali (millimetru/m/ grad c) 0–315 grad c | ko-eff medju ta' espansjoni termali (millimetru/m/ grad c) 0–100 grad c | ko-eff medju ta' espansjoni termali (millimetru/m/ grad c) 0–538 grad c | sħana speċifika 0-100 grad c (j/kg.k) | konduttività termali f'100 grad c (w/mk) | konduttività termali f'500 grad c (w/mk) | resistività tal-elettrika (nω.m) |
|---|---|---|---|---|---|---|---|---|---|
| 316 | 193 | 8000 | 16.2 | 15.9 | 17.5 | 500 | 16.3 | 21.5 | 74 |
Ċart tal-Piż ta' ASME SA 269 316 Bright Annealed Tube
| Dija ta 'barra f'pulzieri | 22ga .028" | 18ga .049" | 20ga .035" | 16ga .065" | 14ga .083" | 12ga 0.109" | 25ga .020" | 28ga .010" | 13ga .095" | 11ga .120" | 9ga .148" | 10ga .134" |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 1 /2 | 8400 | 14700 | 10500 | 19500 | 24900 | 6000 | 28500 | |||||
| 0.1411 | 0.236 | 0.1738 | 0.302 | 0.3696 | 0.1025 | 0.4109 | ||||||
| 5/8 | 6725 | 11750 | 8400 | 15600 | 19925 | 4800 | 22800 | |||||
| 0.1785 | 0.3014 | 0.2205 | 0.3888 | 0.4805 | 0.1292 | 0.5377 | ||||||
| 3/4 | 5600 | 9800 | 7000 | 13000 | 16600 | 21800 | 4000 | 19000 | 24000 | |||
| 0.2159 | 0.3668 | 0.2673 | 0.4755 | 0.5913 | 0.7462 | 0.1559 | 0.6646 | 0.8074 | ||||
| 7/8 | 4800 | 8400 | 6000 | 11150 | 14250 | 18675 | 3425 | 16275 | 20570 | |||
| 0.2533 | 0.4323 | 0.314 | 0.5623 | 0.7021 | 0.8917 | 0.1826 | 0.7914 | 0.9676 | ||||
| 1 | 4200 | 7350 | 5250 | 9750 | 12450 | 16350 | 3000 | 14250 | 18000 | 22200 | 20100 | |
| 0.2907 | 0.4977 | 0.3607 | 0.6491 | 0.8129 | 1.037 | 0.2093 | 0.9182 | 1.128 | 1.347 | 1.251 | ||
| 1 -1 /4 | 3350 | 5875 | 4200 | 7800 | 9950 | 13075 | 11400 | 14400 | 17750 | 16075 | ||
| 0.3654 | 0.6285 | 0.4542 | 0.8226 | 1.034 | 1.328 | 1.172 | 1.448 | 1.742 | 1.612 | |||
| 1 -3/8 | 3050 | 5350 | 3825 | 7100 | 9050 | 11900 | 10350 | 13100 | 16150 | 14625 | ||
| 0.4028 | 0.6939 | 0.5009 | 0.9094 | 1.145 | 1.474 | 1.299 | 1.608 | 1.939 | 1.793 |
Tolleranza Standard ta 'ASTM A269
| Nru. | Daqs, Dijametru ta' Barra, in. | Varjazzjonijiet permissibbli fid-dijametru ta' barra, pulzieri (mm) | Varjazzjonijiet permissibbli fil-Ħxuna tal-Ħitan,% | Varjazzjonijiet permissibbli fit-Tul tal-Qtugħ, pulzieri (mm) | Tubi b'ħitan irqaq | |
| Fuq | Taħt | |||||
| 1 | Sa ½[13] | ±0.005(0.13) | ±15 | ⅛(3.2) | 0 | ... |
| 2 | ½ sa 1½, eskluż | ±0.005(0.13) | ±10 | ⅛(3.2) | 0 | inqas minn 0.065 pulzieri (1.65 mm) nominali |
| 3 | 1½ sa 3½, eskluż | ±0.010(0.25) | ±10 | 3/16(4.8) | 0 | inqas minn 0.095 pulzieri (2.41 mm) nominali |
| 4 | 3½ sa 5½, eskluż | ±0.015(0.38) | ±10 | 3/16(4.8) | 0 | inqas minn 0.150 pulzieri (3.81 mm) nominali |
| 5 | 5½ sa 8, eskluż | ±0.030(0.76) | ±10 | 3/16(4.8) | 0 | inqas minn 0.150 pulzieri (3.81 mm) nominali |
| 6 | 8 sa 12, eskluż | ±0.040(1.01) | ±10 | 3/16(4.8) | 0 | inqas minn 0.200 pulzieri (5.08 mm) nominali |
| 7 | 12 sa 14, eskluż | ±0.050(1.26) | ±10 | 3/16(4.8) | 0 | inqas minn 0.220 pulzieri (5.59 mm) nominali |
X'inhi l-ħruxija tipika tal-wiċċ (Ra) tat-tubi ASTM A269 TP316 BA?
Il-ħruxija interna u esterna tipika ta 'tubi temprat qawwi (BA) hija ġeneralment madwar Ra < 0.5 μm (20 μin). Għal applikazzjonijiet li jeħtieġu purità ogħla bħal fl-industriji tas-semikondutturi jew tal-gass ultra-pur il-valur Ra jista' jitnaqqas aktar għal taħt 0.25 μm permezz ta' electropolishing (EP) sussegwenti.
Applikazzjonijiet:
Tubi ta' Kontroll u Strumentazzjoni.
Kromatografija u tagħmir tal-laboratorju.
Ipproċessar Farmaċewtiku u Biotech.
Sistemi ta' kunsinna ta' gass semikondutturi.
Linji idrawliċi tal-baħar u offshore.
A269 Grad TP316 Cold Drawn Tube Seamless Kodiċi HS
| KODIĊI HS | 73044100 |
|---|
Il-prodotti kollha tagħna jgħaddu minn spezzjoni individwali f'konformità ma 'standards speċifikati qabel l-ippakkjar. Dawk biss li jgħaddu mill-ispezzjoni huma ppakkjati skont il-kriterji tal-esportazzjoni.
Flaring Test
Ittestjar Mekkaniku
Ittestjar Kimiku
Test tal-Iċċattjar
Ittestjar PMI
Ittestjar tal-ebusija

Kunsinna u Ippakkjar
Il-prodotti kollha tal-prodotti tagħna jistgħu jiġu ttrasportati b'diversi mezzi, bħat-tbaħħir sħiħ tal-kontejners, inqas minn tbaħħir tat-tagħbija tal-kontejners, merkanzija bl-ajru, eċċ Il-kumpanija tagħna se tifformula l-aħjar pjan ta 'trasport għal kull ordni biex tiffranka l-ispejjeż tal-akkwist tal-klijenti.