Kompożizzjoni Kimika
| Element | Kompożizzjoni (%) |
|---|---|
| Karbonju (C) | ≤ 0.08 |
| Manganiż (Mn) | ≤ 2.00 |
| Silikon (Si) | ≤ 1.50 |
| Fosfru (P) | ≤ 0.045 |
| Kubrit (S) | ≤ 0.030 |
| Kromju (Cr) | 24.0 - 26.0 |
| Nikil (Ni) | 19.0 - 22.0 |
| Nitroġenu (N) | ≤ 0.10 |
| Ħadid (Fe) | Bilanċ |
⚙️ Proprjetajiet Mekkaniċi
| Proprjetà | Valur |
|---|---|
| Qawwa tat-tensjoni (Temperatura tal-Kamra) | ≥ 515 MPa |
| Qawwa tar-Rendiment (0.2% Offset) | ≥ 205 MPa |
| Titwil (gejġ ta' 50mm) | ≥ 40% |
| Ebusija (Brinell) | ≤ 217 HB |
| Ebusija (Rockwell B) | ≤ 95 HRB |
| Enerġija tal-Impatt (Charpy V-talja) | ≥ 120 J |
| Modulu ta' Young | 200 GPa |
| Limitu tal-Għeja (107ċikli) | 240 MPa |
🔬 Proprjetajiet Fiżiċi
| Proprjetà | Valur |
|---|---|
| Densità | 7.98 g/ċm³ |
| Punt tat-tidwib | 1400-1450°C |
| Konduttività Termali (20°C) | 14.2 W/m·K |
| Koeffiċjent ta' Espansjoni Termali (20-100°C) | 14.4×10-6/K |
| Koeffiċjent ta' Espansjoni Termali (20-1000°C) | 18.0×10-6/K |
| Kapaċità Speċifika tas-Sħana | 500 J/kg·K |
| Reżistività Elettrika (20°C) | 0.78 µΩ·m |
| Permeabilità manjetika | 1.02 µH/m (Mhux-manjetiku) |
| Proporzjon ta' Poisson | 0.27-0.30 |