Kompożizzjoni Kimika
Il-kompożizzjoni kimika tal-materjal SS 410 hija elenkata fit-tabella li ġejja bbażata fuq analiżi fonduta.
Datasheet 1, It-tabella hawn taħt turi l-kompożizzjoni tal-istainless steel AISI 410.
| Tip 410 Kompożizzjoni Kimika, % | ||||||||
| ASTM / SAE | AISI (UNS) | C | Si, ≤ | Mn, ≤ | P, ≤ | S, ≤ | Cr | Ni, ≤ |
| ASTM A276/A276M | 410 (UNS S41000) | 0.08-0.15 | 1.00 | 1.00 | 0.040 | 0.030 | 11.5-13.5 | – |
| ASTM A580/A580M | 0.15, ≤ | 1.00 | 1.00 | 0.04 | 0.03 | 11.5-13.5 | – | |
| ASTM A959 | ||||||||
| ASTM A479/A479M | ||||||||
| ASTM A314 | ||||||||
| ASTM A240/A240M | 0.08-0.15 | 1.00 | 1.00 | 0.04 | 0.03 | 11.5-13.5 | 0.75 | |
| ASTM A473 | 0.15, ≤ | |||||||
| SAE J405 | 0.15, ≤ | |||||||
Noti:
ASTM A276/A276M: Speċifikazzjoni Standard għal Bars u Forom ta 'Stainless Steel
ASTM A240/A240M: Kromju u Kromju-Pjanċa, Folja u Strixxa ta' l-Azzar li ma jsaddadx tan-nikil għal Reċipjenti ta' Pressjoni u għal Applikazzjonijiet Ġenerali
ASTM A580/A580M: Stainless Steel Wajer
ASTM A479/A479M: Vireg u Forom ta 'l-Azzar li ma jsaddadx għall-Użu f'Boilers u Reċipjenti Oħra ta' Pressjoni
ASTM A959: Gwida Standard għall-Ispeċifikazzjoni ta' Kompożizzjonijiet ta' Grad Standard Armonizzati għal Azzar Stainless Wrought
ASTM A473: Forġar tal-Azzar li ma jsaddadx
ASTM A314: Speċifikazzjoni Standard għal Billets ta 'Stainless Steel u Bars għall-Forġa
SAE J405: Kompożizzjoni Kimika ta 'SAE Wrought Stainless Steels
Ibgħat l-inkjesta