UNS N08904 904L Stainless Steel Tube Seamless 1/8 sa 10 OD DIN1.4539 Stainless Steel Pipe
Mar 23, 2026
Ħalli messaġġ



Speċifikazzjonijiet:
Gradi tal-istainless steel 904 l: 00 cr20ni25mo4. 5 cu/UNS: N08904 / EN: 1.4539
Firxiet ta 'kompożizzjoni ta' azzar li ma jissaddadx ta 'grad 904L
|
Grad |
C |
Mn |
Si |
P |
S |
Cr |
Mo |
Ni |
Cu |
|
|
904L |
min. max. |
- 0.02 |
- 2 |
- 1 |
- 0.045 |
- 0.035 |
19 23 |
4 5 |
23 28 |
1 2 |
Proprjetajiet mekkaniċi tal-istainless steel ta 'grad 904L
|
Grad |
Qawwa tat-tensjoni (MPa) min |
Qawwa tar-Rendiment 0.2% Prova (MPa) min |
Titwil (% f'50mm) min |
Ebusija |
|
|
Rockwell B (HR B) |
Brinell (HB) |
||||
|
904L |
490 |
220 |
36 |
70-90 tipiku |
150 |