X'inhu 440 Stainless Steel?
Feb 24, 2026
Ħalli messaġġ



Materjal Ekwivalenti ta '440 Stainless Steel Plate
Azzar li ma jsaddadx 440A:
Ekwivalenti għal AISI 440A, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5631, AMS 5632, AMS 5633, AMS 5634, AMS 5880, MIL 5880, MIL 5880, SAIL (51440A)
Gradi simili: 7Cr17, 7Cr17MoV, X70CrMo15
440B Stainless Steel:
Ekwivalenti għal AISI 440B, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5631, AMS 5632, AMS 5633, AMS 5634, AMS 5880, MIL 5880, MIL 5880, SAIL (51440B)
Gradi simili: 9Cr18, 9Cr18Mo, X90CrMoV18
440C Stainless Steel:
Ekwivalenti għal AISI 440C, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5630, AMS 5880, MIL-S-862, SAE J405 (51440C)
Gradi simili: 9Cr18MoV, X105CrMo17
440 Stainless Steel Plate Kompożizzjoni Kimika (%)
| Grad | C | Si | Mn | S | P | Cr | Ni | Mo |
|---|---|---|---|---|---|---|---|---|
| 440A | 0.60~0.75 | Inqas minn jew ugwali għal 1 | Inqas minn jew ugwali għal 1 | Inqas minn jew ugwali għal 0.030 |
Inqas minn jew ugwali għal 0.040 |
16.00-18.00 | – | Inqas minn jew ugwali għal 0.75 |
| 440B | 0.85-0.95 | Inqas minn jew ugwali għal 1 | Inqas minn jew ugwali għal 1 | Inqas minn jew ugwali għal 0.030 | Inqas minn jew ugwali għal 0.035 | 16.00-18.00 | Inqas minn jew ugwali għal 0.60 | Inqas minn jew ugwali għal 0.75 |
| 440C | 0.95 – 1.20 | Inqas minn jew ugwali għal 1 | Inqas minn jew ugwali għal 1 | Inqas minn jew ugwali għal 0.030 | Inqas minn jew ugwali għal 0.040 | 16.00-18.00 | – | Inqas minn jew ugwali għal 0.75 |
Proprjetajiet Mekkaniċi
| Proprjetà | 440A | 440B | 440C |
|---|---|---|---|
| Ebusija (Rockwell C) | 56-59 HRC | 57-60 HRC | 58-62 HRC |
| Qawwa tat-tensjoni (MPa) | 760-820 | 760-840 | 760-820 |
| Qawwa tat-tensjoni (MPa) | 450-600 | 450-600 | 450-600 |
| It-titwil fil-waqfa (%) | 20-25 | 15-20 | 10-15 |
| Modulu ta' Elastiċità (GPa) | 200 | 200 | 200 |
Proprjetajiet Fiżiċi
| Proprjetà | 440A | 440B | 440C |
|---|---|---|---|
| Densità (g/cm³) | 7.65 | 7.75 | 7.75 |
| Konduttività Termali (W/m·K) | 24 | 24 | 24 |
| Kapaċità Speċifika tas-Sħana (J/kg·K) | 460 | 460 | 460 |
| Reżistenza Elettrika (μΩ·cm) | 60 | 60 | 60 |
| Koeffiċjent ta' Espansjoni Termali (μm/m·K) | 10.4 | 10.4 | 10.4 |