| SUS316 | SS316 | |
|---|---|---|
| 16–18% | 16–18% | |
| 10–14% | 10–14% | |
| 2–3% | 2–3% | |
| <= 0.08% | <= 0.08% | |
| <= 2% | <= 2% | |
| <= 1% | <= 1% | |
| <= 0.045% | <= 0.045% | |
| <= 0.03% | <= 0.03% | |
| <= 0.10% | <= 0.10% | |
What is the difference between SUS304 and SUS316?
The main difference is that SUS316 contains 2-3% molybdenum, which provides superior corrosion resistance compared to SUS304, especially against chlorides and acidic conditions. Because of this added element, SUS316 is more expensive and better suited for marine and chemical applications, while SUS304 is a more economical choice for less corrosive environment.
What is the difference between SUS316L and SUS316?
The main difference is that SUS316L has a lower carbon content than SUS316, making it more resistant to intergranular corrosion, especially after welding. This makes SUS316L the preferred choice for applications that require welding, while SUS316 may have slightly higher strength properties. Both grades share similar corrosion resistance due to their high molybdenum content.
If you have project requirements for SUS316 stainless steel, we welcome your order. GNEE has a large inventory of popular products for you to choose from. It can be processed into various practical product forms, including plates, coils, tubes, bars, wires, etc. For detailed chemical composition information and free samples, please contact our factory immediately. We offer competitive prices and excellent service.Email: info@gneestainless.com
Testing and Documentation: Factory test certificate, EN 10204 3.1, chemical report, mechanical report, destructive testing report, non-destructive testing report, PMI test report, visual inspection report, third-party inspection report, NABL certified laboratory report.