ASTM A213 TP304L Stainless Steel Boiler Tube
Grad tal-Materjal: TP304L
Grad Ekwivalenti: EN 1.4307 / X2CrNi18-9 / SUS304L
Proċess ta 'Manifattura: Seamless Cold Drawn / Cold Rolled
Kundizzjoni tal-Provvista: Kundizzjoni Ittemprata u Ttrattata bis-Sħana
Dijametru ta 'barra (OD): 6.0 mm - 127 mm (daqsijiet tad-dwana disponibbli)
Ħxuna tal-ħajt: 0.5 mm - 12.7 mm
Tul: 3000 mm / 6000 mm / Tul Personalizzat
Finish tal-wiċċ: imnaddfin, ittemprat qawwi (BA), illustrat
Ċertifikazzjoni:EN 10204 3.1 MTC, Rapport PMI, Rapport tat-Test Mekkanika
ASTM A213 TP304L Stainless Steel Boiler Tube fornitur
ASTM A213 TP304L Stainless Steel Boiler Tube huwa tubu ta 'l-istainless steel awstenitiku b'livell baxx ta' karbonju applikat f'bojlers, skambjaturi tas-sħana, kondensaturi, u tagħmir għat-trasferiment tas-sħana b'temperatura għolja. Meta mqabbel ma 'l-istainless steel standard 304, TP304L għandu kontenut ta' karbonju aktar baxx (C Inqas minn jew ugwali għal 0.030%), li effettivament inaqqas ir-riskju ta 'korrużjoni intergranulari ikkawżata minn preċipitazzjoni tal-karbur tal-kromju waqt l-iwweldjar u l-operazzjoni f'temperatura għolja. Huwa adattat b'mod speċjali għal tagħmir ta 'pressjoni li jeħtieġ tħaddim stabbli fit-tul f'temperaturi elevati. Meta mqabbel ma 'TP316L, 304L jipprovdi effiċjenza aħjar fl-ispiża f'ambjenti kemmxejn korrużivi, sistemi ta' fwar b'temperatura għolja, u applikazzjonijiet ta 'skambjatur tas-sħana sensittivi għall-ispiża.
It-tubi ta 'l-istainless steel ASTM A213 TP304L li nipprovdu għandhom kontenut ta' karbonju ta 'Inqas minn jew ugwali għal 0.03%, li jippermettu komponenti wweldjati biex jevitaw korrużjoni intergranulari mingħajr trattament tas-sħana addizzjonali wara l-iwweldjar. Dan il-materjal huwa adattat għal strutturi tal-bojlers iwweldjati kumplessi, b'temperatura ta 'servizz kontinwu sa 538 grad u reżistenza għat-temperatura massima għal żmien qasir sa 700 grad.
It-tubi tal-iskambjatur tas-sħana tal-istainless steel ASTM A213 TP304L jipprovdu kapaċità ta 'reżistenza għall-pressjoni sa 10 MPa, li jissodisfaw ir-rekwiżiti ta' sistemi tal-fwar bi pressjoni għolja fil-bojlers tal-impjant tal-enerġija. Il-ħruxija tal-wiċċ hija kkontrollata f'Ra Inqas minn jew ugwali għal 0.8 μm, li tgħin biex titnaqqas l-adeżjoni tal-iskala u ttejjeb l-effiċjenza tat-trasferiment tas-sħana. Dawn it-tubi jistgħu jirreżistu l-korrużjoni mill-impuritajiet tal-ilma tal-bojler (bħal Cl⁻ u SO₄²⁻) u ambjenti tal-fwar b'temperatura għolja. Huma għaddew mit-test tal-korrużjoni intergranulari ASTM A262, u wara t-trattament tal-pickling u passivazzjoni tal-wiċċ, flimkien ma 'aktar minn 1000 siegħa ta' ttestjar tal-isprej tal-melħ, jipprovdu ħajja ta 'servizz estiża għal sistemi tal-bojler.


Jekk qed takkwista jew taħdem ma 'dawn it-tubi, għarrafni:
• Liema dijametru ta 'barra u ħxuna tal-ħajt (jew skeda) għandek bżonn?
• Qed tfittex eżekuzzjoni mingħajr saldatura jew iwweldjati?
• X'inhuma t-temperatura operattiva u l-pressjoni tas-sistema tiegħek?
ASTM A213 TP304L Tubi tal-kondensatur tal-istainless steel Speċifikazzjoni
Kompożizzjoni Kimika (wt%)
| Element | C | Mn | P | S | Si | Cr | Ni | Mo | N |
| Max / Medda | 0.035 | 2.00 | 0.045 | 0.030 | 1.00 | 18.0 – 20.0 | 8.0 – 13.0 | – | – |
Proprjetajiet Mekkaniċi (Soluzzjoni Ittemprat)
| Proprjetà | Rekwiżit ASTM A213 |
| Qawwa tat-tensjoni (Rm) | Iktar minn jew ugwali għal 485 MPa (70 ksi) |
| Qawwa tar-Rendiment (Rp0.2) | Iktar minn jew ugwali għal 170 MPa (25 ksi) |
| Titwil (f'2 pulzieri / 50 mm) | Iktar minn jew ugwali għal 35% |
| Ebusija (HBW) | Inqas minn jew ugwali għal 192 |
| Ebusija (HV) | Inqas minn jew ugwali għal 200 |
| Ebusija (HRB) | Inqas minn jew ugwali għal 90 |
Dimensjonijiet u Tolleranzi tat-Tubu ASTM A213
| Parametru | Firxa |
| Dijametru Intern (ID) | 3.2 mm (⅛") u 'l fuq |
| Dijametru ta' Barra (OD) | 6.35 – 127 mm (¼" – 5") |
| Ħxuna tal-ħajt | 0.4 – 12.7 mm (0.015" – 0.500") |
| Tul | Wieħed każwali / Doppju każwali / Tul maqtugħ (massimu ~ 25,000 mm) |
| Proċess | Seamless (lest bis-sħana jew lest fil-kesħa / miġbud fil-kesħa) |
Varjazzjonijiet permissibbli fl-OD
| Medda OD (mm) | Tolleranza OD (mm) |
| Inqas minn jew ugwali għal 25.4 | ± 0.10 |
| 25.4 – 38.1 | ± 0.15 |
| 38.1 – 50.8 | ± 0.20 |
| 50.8 – 63.5 | ± 0.25 |
| 63.5 – 76.2 | ± 0.30 |
| 76.2 – 101.6 | ± 0.38 |
Tolleranza tal-Ħxuna tal-Ħajt
| Kundizzjoni | Tolleranza |
| OD Inqas minn jew ugwali għal 50.8 mm | −10% (mhux pożittiv) |
| OD > 50.8 mm, WT > 5.6 mm | ±10% tal-ħajt medju |
Tolleranza tat-Tul
| OD (mm) | Tolleranza tat-Tul |
| < 50.8 | +3 mm, 0 |
| Akbar minn jew ugwali għal 50.8 | +5 mm, 0 |
ASTM A213 Daqsijiet tal-Boiler / Heat-Exchanger Tube
| OD (mm) | OD (fi) | WT (mm) | WT (in) | Applikazzjoni Tipika |
| 12.70 | ½" | 1.65 | 0.065" | Tubi tal-kondensatur |
| 15.88 | ⅝" | 1.65 | 0.065" | Tubi tal-kondensatur |
| 19.05 | ¾" | 1.65 | 0.065" | Kondensatur / tubi li jkessħu |
| 19.05 | ¾" | 2.11 | 0.083" | Tubi tas-superheater |
| 25.40 | 1" | 2.11 | 0.083" | Tubi tal-evaporatur |
| 25.40 | 1" | 2.77 | 0.109" | Tubi tas-superheater |
| 31.75 | 1¼" | 2.77 | 0.109" | Tubi economizer |
| 38.10 | 1½" | 3.40 | 0.134" | Evaporatur / superheater |
| 44.45 | 1⅜" | 3.40 | 0.134" | Tubi tas-superheater |
| 50.80 | 2" | 3.40 | 0.134" | Dnabar tal-fwar / headers |
| 60.33 | 2⅜" | 4.19 | 0.165" | Tubi tas-superheater |
| 76.20 | 3" | 4.19 | 0.165" | Economizer / bojler |
| 88.90 | 3½" | 4.19 | 0.165" | Bojler b'dijametru kbir |
| 101.60 | 4" | 5.56 | 0.219" | Linji tal-fwar / kondensat |
| 114.30 | 4½" | 5.56 | 0.219" | Pajpijiet ta' utilità |
| 127.00 | 5" | 5.56 | 0.219" | Headers tal-fwar |
Nota:
Manifatturat bl-użu ta 'proċess mingħajr saldatura (rolling bis-sħana segwit minn tpinġija kiesħa) biex jiġi żgurat korp ta' tubu mingħajr weldjatura;
Tubi miġbudin fil-kesħa (CD) għandhom tolleranzi dimensjonali aktar stretti (tolleranza OD ± 0.10 mm) u finitura tal-wiċċ aktar lixxa, li tagħmilhom l-għażla preferuta għal applikazzjonijiet ta 'kondensatur u skambju tas-sħana ta' preċiżjoni.
Kundizzjoni tal-wiċċ: Kif lest (bright) jew passivat; tipikament, l-ebda trattament tal-wiċċ addizzjonali ma huwa meħtieġ għall-kundizzjonijiet tat-tħaddim tal-bojler.
Applikazzjonijiet tipiċi: Boilers tal-impjanti tal-enerġija, superheaters, economizers, kondensaturi, u skambjaturi tas-sħana, kif ukoll setturi bħall-ipproċessar tal-ikel u farmaċewtiku, polpa u karta, u proċessar kimiku (ambjenti mhux kloruri).
Ħin taċ-Ċomb:
Speċifikazzjonijiet standard (OD 12.7–50.8 mm, WT 1.65–3.40 mm): 7–15-il jum għal oġġetti tal-istokk; ordnijiet mhux standard/personalizzati (ħxuna tal-ħajt speċjali, tul, jew trattament EP): 30-45 jum; ordnijiet ta 'volum kbir (Aktar minn jew ugwali għal 50 tunnellata): 45-60 jum. L-ordnijiet jiġu ssorveljati permezz tal-ERP matul il-proċess kollu, b’rapporti ta’ progress tal-produzzjoni ta’ kull ġimgħa pprovduti; spezzjonijiet minn partijiet terzi (SGS, BV, CCIC) huma appoġġjati.
Spezzjoni tal-Kwalità
Tubi tal-bojler tal-istainless steel ASTM A213 TP304L jgħaddu minn spezzjonijiet ta 'kwalità rigorużi qabel il-ġarr, inkluż analiżi tal-kompożizzjoni kimika, ittestjar tat-tensjoni, ittestjar tal-ebusija, ittestjar idrostatiku, ittestjar tal-kurrent eddy, u kontrolli dimensjonali. Kull tubu jgħaddi minn 100% ittestjar mhux distruttiv biex jiżgura li d-dijametru ta 'barra u t-tolleranzi tal-ħxuna tal-ħajt jikkonformaw mal-istandards ASTM A213; barra minn hekk, huwa pprovdut ċertifikat tal-materjal EN 10204 3.1 biex jiggarantixxi t-traċċabilità tan-numru tas-sħana.






Ippakkjar għall-Esportazzjoni:
It-truf tal-pajpijiet huma ssiġillati b'tappijiet tal-plastik biex jipprevjenu l-kontaminazzjoni, u l-korpi tal-pajpijiet huma mgeżwra f'film PE li ma jgħaddix umdità. Il-qatet (Inqas minn jew ugwali għal 2 tunnellati) huma mwaħħlin b'mod sikur u appoġġjati minn pallets tal-injam jew xtillieri tal-azzar. Il-barra hija protetta minn folja galvanizzata tal-metall jew boroż minsuġa. Għal vjeġġi bil-baħar, karta kontra s-sadid VCI hija inkluża. Il-kundizzjonijiet tal-kontenitur jinżammu f'Inqas minn jew ugwali għal 40 grad u Inqas minn jew ugwali għal 65% RH biex jiżguraw żero sadid jew ħsara mal-wasla.

It-tags Popolari: astm a213 tp304l stainless steel boiler tube, iċ-Ċina astm a213 tp304l stainless steel boiler tube manifatturi, fornituri, fabbrika
You Might Also Like
Ibgħat l-inkjesta








