ASTM A269 TP316L Seamless Bright Annealed Strument Tubing
Forma: tonda
Teknika: Cold Rolled
Trattament tal-wiċċ: Sanded / Mirror / Hairline Brushed
Ħxuna: 0.3-30mm
Dijametru barra: 8-219mm
Tul: 5.8/6m jew Custom
Stokk: fl-istokk
Kampjun: Disponibbli
Pakkett tat-Trasport: Ippakkjar Standard li jistħoqq il-baħar
ASTM A269 TP316L Fornitur tat-tubi tal-istrumenti mingħajr saldatura
GNEE huwa manifattur, esportatur, distributur, stockist, u fornitur magħruf ta 'tubi ittemprati jleqqu ta' l-istainless steel. Il-prodotti tagħna jikkonformaw mal-istandards nazzjonali u internazzjonali tal-kwalità tal-materja prima.
ASTM A269 TP316L tubi ta 'strumenti ttemprati jleqqu mingħajr saldatura li nipprovdu huma pajpijiet mingħajr saldaturi ta' preċiżjoni għolja magħmula minn azzar li ma jissaddadx b'livell baxx ta 'karbonju (C Inqas minn jew ugwali għal 0.03%) tal-grad TP316L standard Amerikan. Ipproċessati permezz ta 'tekniki ta' tpinġija kiesħa u ttemprar qawwi (BA), dawn it-tubi għandhom ħitan ta 'ġewwa u ta' barra lixxi u juru reżistenza għall-korrużjoni eċċellenti, li jagħmluhom partikolarment adattati għal oqsma b'rekwiżiti stretti ta 'ndafa, bħal gassijiet ta' purità għolja, apparat mediku, u strumenti elettroniċi.

TP316L tubi ttemprati jleqqu mingħajr saldatura jikkonformaw ma 'standards inklużi ASTM A269 u ASME SA-312. Speċifikazzjonijiet komuni jinkludu dijametri ta 'barra ta' 1/8''–4'' (metrika 3–219 mm) u ħxuna tal-ħajt ta '0.035''–0.2'' (metrika 0.5–5 mm), bi ħruxija tal-ħajt ta' ġewwa fina daqs Ra Inqas minn jew ugwali għal 0.05μm. Dawn it-tubi jintużaw ħafna f'industriji bħal kimiċi, semikondutturi, u ikel u xorb għat-trasport ta 'midja korrużiva jew fluwidi ta' purità għolja.

Speċifikazzjoni
| Grad | 316 |
|---|---|
| Speċifikazzjonijiet | ASTM A269 / ASME SA269 |
| O.D. | Fornitur ta 'Wweldjat/ ERW minn 10 sa 114.3 millimetru OD Seamless: 6 sa 114.3 millimetru OD |
| Formola | Forma "U", Pjazza, Coils Pan Kejk, Coiled, Rettangolari, Round, Tubu Idrawliku. |
| Tmiem | Invitati, Beveled, bil-kamin, Plain |
| Tul | Single Random, Double Random, Aqta għat-tul |
| Skeda Firxiet tal-Ħxuna | SCH XS, SCH 40, SCH 80S, SCH 5, SCH 80, SCH XXS, SCH 160, SCH10, L-iskedi kollha |
| Tip | Iwweldjati|CDW|ERW|DOM|Bla xkiel|Fabbrikat|CEW |
| Finish tal-wiċċ | 2B, No.1, No.4, No.8 Mirror Finish |
| Daqsijiet | 5.0 milimetru - 1219.2 milimetru |
Struttura Kimika ta' ASTM A269 316 Tube
| GRADI | UNS | C | Mn | P | S | Si | Cr | Ni |
| ASME SA269 316 | S31600 | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 8.0-13.0 |
Tabella tal-Proprjetajiet Mekkaniċi tat-Tubi tat-Tip 316 ASTM A269
| Materjal | Saħħan | Temperatura | Qawwa tat-tensjoni | Qawwa tar-Rendiment | Titwil %, Min |
| Trattament | Min.º F (º C) | Ksi (MPa), Min. | Ksi (MPa), Min. | ||
| TP316 | Soluzzjoni | 1900 (1040) | 70(485) | 25(170) | 35 |
Tabella tad-Daqs Standard ASTM A269 (pulzieri)
Disponibbli f'tulijiet ta '6 metri (20ft) jew koljaturi kontinwi.
| OD (pulzier) | WT (pulzier) | WT (mm) | Pressjoni Max tax-Xogħol (Stima)* |
| 1/16" | 0.010" | 0.25 | 5000+ psi |
| 1/8" | 0.028" | 0.71 | 8500 psi |
| 1/4" | 0.035" | 0.89 | 5100 psi |
| 1/4" | 0.049" | 1.24 | 7500 psi |
| 3/8" | 0.035" | 0.89 | 3300 psi |
| 1/2" | 0.049" | 1.24 | 3500 psi |
| 1/2" | 0.065" | 1.65 | 4700 psi |
| 3/4" | 0.065" | 1.65 | 3000 psi |
ASTM A269 Gr TP316 Seamless Tube Lista tal-Prezzi
| Prodott | Prezz |
|---|---|
| ASTM A269 TP316 6MM Stainless Steel Hollow Condenser SUS Pajp | $2,250.00 - $2,570.00/Tunnellata Metrika |
| ASTM A269 TP316/L SMLS U-BAND Tube għal Heat Exchanger | $3.00/ Kilogramma |
| Pajpijiet ASTM A269 SS316, 1/16" sa 2" OD | $1.00 - $14.90/Metru |
| ASTM A269 TP316l Dijametru Żgħir Stainless Steel Boiler Pipe | $4.65 - $5.75/Metru |
316L BA tubi appoġġ liwi?
Yes. Our ASTM A269 TP316L BA tubing is fully annealed with an elongation >35% u ebusija<90 HRB, making it perfect for high-precision bending without cracking or kinking.
spezzjoni
Ittestjar tal-flanġ u tal-flare, ittestjar tal-iċċattjar invers, ittestjar tal-ħruxija, ittestjar idrostatiku/pnewmatiku, ittestjar tal-kurrent eddy (NDT), verifika tal-finitura tal-wiċċ, spezzjoni dimensjonali, ċertifikazzjoni tal-materjal.



Stainless Steel 316 TubeFabbrika
Servizzi ta' Valur Miżjud:
* ** Ċanfrin: ** Jipprovdi ċanfrin preċiż tat-tarf tal-pajp għall-iwweldjar fuq il-post.
* **Threading:** Joffri konnessjonijiet bil-kamin NPT jew BSP.
* ** Qtugħ: ** Juża srieraq tal-faxxa jew qtugħ bil-lejżer b'tolleranzi ta 'tul ikkontrollati fi ħdan ± 1mm.
* **Spezzjoni:** Jappoġġja l-ittestjar spettrali PMI, l-ittestjar ultrasoniku (UT), l-ittestjar tal-kurrent eddy (ET), u l-ispezzjoni ta 'parti terza.


Ippakkjar u Immarkar
L-ippakkjar għandu jkun f'qatet jew ċestuni tal-injam laminati, imgeżwer fil-plastik, u għandhom jittieħdu miżuri protettivi xierqa biex tiġi żgurata l-kapaċità għall-baħar għat-trasport jew kif meħtieġ.
L-immarkar għandu jikkonforma mad-dispożizzjonijiet tal-ispeċifikazzjonijiet A1016/A1016M u għandu jinkludi jekk il-pajpijiet humiex maħduma bis-sħana jew maħduma bil-kesħa, inklużi iżda mhux limitati għal: standard, grad, daqs, numru tal-forn, u numru tal-lott.