UNS S30908 Stainless Steel – High-Chromium Heat-Resistant Utility Alloy304L Stainless Steel Sheet for Chemical Tank Linings304L Stainless Steel Coil for Petrochemical Pipelines

Kompożizzjonijiet Kimiċi

Element

C

Mn

Si

Cr

Ni

P

S

Fe

Medda ta' Kompożizzjoni (%) 0.08 – 0.15 1.00 max 1.00 max 11.50 – 13.50 0.75 max 0.04 max 0.03 max Bilanċ

Proprjetajiet Mekkaniċi

Proprjetà Mekkanika

Valur (Metriku)

Valur (Imperjali)

Qawwa tat-tensjoni 480 – 620 MPa 70 – 90 ksi
Qawwa tar-Rendiment 275 – 450 MPa 40 – 65 ksi
Ebusija Brinell (HB) 170 – 201 HB 170 – 201 HB
Ebusija Rockwell (HRC) 20 – 30 HRC 20 – 30 HRC
Ebusija Vickers (HV) 180 – 230 HV 180 – 230 HV
Titwil 20% – 25% 20% – 25%
Modulu Elastiku 200 GPa 29 x 10³ ksi