ASTM A240 Grad 310S Hot Rolled Stainless Steel Plate Imrattab U Imneħħija
Mar 23, 2026
Ħalli messaġġ



|
Speċifikazzjoni |
201, 202, 301, 304, 304j1, 304l, 321, 309s, 310s, 2205, 409l, 410, 410s, 420, 420j1, 420j2, 493, 4, 493, 4, 49 444, eċċ |
|
Komodità |
Austenitic, Ferritic, Martensitic, Duplex, Cold rolled, Hot rolled |
|
Tul |
1000mm-11000mm jew bħala l-ħtieġa tal-klijent |
|
Wisa' |
10-2000mm |
|
wiċċ |
N0.1, N0.2, N0.3, N0.4, N0.5, N0.6, N0.7, N0.8, 2D, 2B, HL, BA, 6K, 8K, eċċ |
|
Ħin tal-kunsinna |
Fi żmien 7-15-il jum |
|
Xenarji ta' applikazzjoni |
Arkitettura, kostruzzjoni, bini, Oġġetti tal-kċina |
|
pajjiż tal-oriġini |
Jiangsu, iċ-Ċina |
|
Sengħa |
hot rolled, cold rolled |
|
Avviż |
Nistgħu wkoll nagħmlu materjali oħra |
Proprjetajiet Creep
Proprjetajiet Tipiċi Creep
|
Temperatura |
Creep Strain (MPa) |
Creep Rapture (MPa) |
|||||
|---|---|---|---|---|---|---|---|
| grad | grad F | 1000 H | 10000 H | 100000 H | 1000 H | 10000 H | 100000 H |
| 600 | 1112 | 120 | 100 | 40 | 200 | 140 | 80 |
| 700 | 1292 | 50 | 35 | 20 | 80 | 45 | 20 |
| 800 | 1472 | 20 | 10 | 8 | 35 | 20 | 8 |
| 900 | 1652 | 10 | 6 | 3 | 15 | 10 | 5 |
| 1000 | 1832 | 5 | 3 | 1.5 | 9 | 4 | 2 |
Analiżi Kimika
Piż % (il-valuri kollha huma massimi sakemm firxa ma tkunx indikata mod ieħor)
| Element | 310 | 310S | 310H |
|---|---|---|---|
| Kromju | 24.0 min.-26.0 max. | 24.0 min.-26.0 max. | 24.0 min.-26.0 max. |
| Nikil | 19.0 min.-22.0 max. | 19.0 min.-22.0 max. | 19.0 min.-22.0 max. |
| Karbonju | 0.25 | 0.08 | 0.04 min. - 0.10 max. |
| Manganiż | 2.00 | 2.00 | 2.00 |
| Fosfru | 0.045 | 0.045 | 0.045 |
| Sulfer | 0.030 | 0.030 | 0.030 |
| Silikon | 1.50 | 1.50 | 0.75 |
| Ħadid | Bilanċ | Bilanċ | Bilanċ |
Ibgħat l-inkjesta