AISI 904L 20mmx4ftx8ft Inox UNS N08904 1.4539 S39042 Hot Rolled Stainless Steel Plate

Mar 23, 2026

Ħalli messaġġ

304L Stainless Steel Sheet for Chemical Tank Linings304 Stainless Steel Sheet for Medical DevicesUNS S31635 Stainless Steel – Titanium-Stabilized High-Temp 316 Alloy

Deskrizzjoni

Materjal: Stainless Steel 904L Irfinar: Trab Miksija, Mhux Miksija, Galvanizzat
Tip: Fjura Kettle/bexxiexa, Kitts Propagatur Tip tal-metall: Stainless Steel
Stil: Morden Sempliċi Kundizzjoni tal-Użu: ART
Użat Ma': Fjura/Pjanti Aħdar Daqs: Daqs Personalizzat, bħala Talba Tiegħek
Forma: Ċatt Ħxuna: 1.5-3 Mm Jew Personalizzat

 

Kompożizzjoni Kimika

 

Grad C Mn Si P S Cr Mo Ni Cu
904L

min.

max.

-

0.02

-

2

-

1

-

0.045

-

0.035

19

23

4

5

23

28

1

2

 

Proprjetajiet

 

Grad Qawwa tat-tensjoni (MPa) min Qawwa tar-Rendiment 0.2% Prova (MPa) min Titwil (% f'50mm) min Ebusija
Rockwell B (HR B) Brinell (HB)
904L 490 220 36 70-90 tipiku 150